This took forever to get right, but all my filament dryboxes are at 10% and I can’t get it any lower.
minus-squarejokeyrhyme@lemmy.mllinkfedilinkEnglisharrow-up3·7 days agofor some filament, at least PLA and PETG, you don’t want to filament entering the extruder to be too warm because it can soften and cause jams / under-extrusion
for some filament, at least PLA and PETG, you don’t want to filament entering the extruder to be too warm because it can soften and cause jams / under-extrusion